25mm GH2747 Nickel Superalloy Round Bar with 1250°C Oxidation Resistance for High-Temp Furnace Parts

25mm GH2747 Nickel Superalloy Round Bar with 1250°C Oxidation Resistance for High-Temp Furnace Parts

Brand Name: DLX
Model Number: GH2747
MOQ: 10 kg
Payment Terms: L/C,D/A,D/P,T/T,VTB
Supply Ability: 1200 tons per month
Detail Information
Place of Origin:
China Jiangsu
Certification:
CE,ROHS
Packaging Details:
Spool package with Carton box, Coil package with polybag, Wooden case package
Supply Ability:
1200 tons per month
Highlight:

GH2747 nickel alloy round bar

,

25mm high-temp furnace bar

,

nickel superalloy furnace parts

Product Description

Explore high-purity 25mm GH2747 nickel-based superalloy round bars designed for superior structural reliability, exceptional high-temperature oxidation resistance up to 1250°C, and stringent dimensional accuracy in thermal processing applications.

GH2747 superalloy round bar Customized service available

Product Overview

GH2747 is an advanced Fe-Ni-Cr based precipitation-hardening superalloy formulated with optimized additions of aluminum and titanium to form a stable intermetallic strengthening network. Operating in prolonged thermal exposure zones up to 1100°C–1250°C, the alloy forms a dense, self-healing chromium-aluminum oxide protective scale that prevents rapid oxidation, gas carburization, and thermal degradation.

The 25mm diameter solid round bar is hot-forged and precision-machined, undergoing strict solution heat treatment to balance tensile strength with elongation. With enhanced resistance to thermal shock and cycle-induced microcracking, GH2747 serves as an ideal material upgrade where standard heat-resistant stainless steels and basic nickel alloys experience premature thermal failure.

GH2747 superalloy round bar details

Technical Specifications

Table 1: Nominal Chemical Composition of GH2747 Superalloy (%)

Element Nickel Chromium Aluminum Titanium Iron Manganese Silicon Carbon Phosphorus Sulfur Boron Cerium
Symbol Ni Cr Al Ti Fe Mn Si C P S B Ce
wt. % 45.00–49.00 18.00–21.00 2.10–2.80 0.80–1.40 Balance ≤ 0.70 ≤ 0.70 ≤ 0.10 ≤ 0.015 ≤ 0.012 ≤ 0.008 ≤ 0.030


Table 2: Physical & Mechanical Properties of GH2747 Round Bar

Property Testing Condition / State Value / Requirement
Density Room Temperature 7.92 g/cm³
Melting Point Range Solidus – Liquidus 1340°C – 1390°C
Max Operating Temperature Continuous / Intermittent Up to 1200°C (Intermittent: 1250°C)
Tensile Strength (Rm) Room Temperature ≥ 680 MPa
Yield Strength (Rp0.2) Room Temperature ≥ 340 MPa
Elongation at Break (A) Room Temperature ≥ 25%
Hardness Solution Annealed State ≤ 220 HBW

Table 3: Dimensional Tolerances & Delivery Conditions (25mm Round Bar)

Specification Parameter Technical Standard & Range
Nominal Diameter 25.0 mm
Diameter Tolerance High-precision class (±0.04 mm to ±0.08 mm via centerless grinding)
Straightness ≤ 1.0 mm/m
Surface Finish Options Centerless Ground / Peeled / Smooth Turned (Ra≤0.8 μm optional)
Delivery Lengths 1,000 mm – 6,000 mm (Custom precision cut-to-length supported)
Internal Quality Inspection 100% Full-length Ultrasonic Testing (UT) & Eddy Current Testing

Core Performance

  • Superior High-Temperature Oxidation Resistance (1250°C): Forms an ultra-adherent protective oxide layer under prolonged high-temperature exposure, preventing deep scaling and premature wall thinning in continuous furnace atmospheres.
  • Robust Thermal Shock & Fatigue Durability: Maintains microstructural stability through repeated rapid heating and cooling cycles without surface cracking or embrittlement.
  • Controlled Metallurgical Purity & Cleanliness: Double-refined through VIM+ESR melting technology to ensure ultra-low gas content (O, N, H) and minimal non-metallic inclusions, maximizing fatigue life under cyclic loads.
  • Exceptional Machinability & Weldability: Features consistent plasticity for precision turning, milling, and thread cutting, with dependable joint integrity under specialized industrial gas shielding welding procedures.
  • Tight Dimensional & Straightness Tolerances: Processed with automated straightening and centerless precision grinding to guarantee seamless feeding into CNC turning centers and automated manufacturing lines.

GH2747 superalloy round bar comparison

Industrial Applications

  • Industrial Heat Treatment & Thermal Furnaces: Radiant heater tubes, heating element support fixtures, furnace rollers, carrier racks, and charging baskets subject to continuous high heat.
  • Petrochemical & Gas Processing: Thermocouple protection wells, high-temperature valve stems, reactor internal brackets, and catalytic combustion chamber components.
  • Aerospace & Gas Turbine Systems: Combustion chamber structural rings, flame stabilizers, transition duct supports, and thermal guide vanes.
  • Power Generation & Metallurgical Equipment: Flue gas dampers, hot gas duct deflectors, burner nozzles, and high-temperature fastener blanks.

GH2747 superalloy round bar application field

Why Source From DLX

  • 1,200 Tons Monthly Capacity: Backed by a dedicated production complex yielding over 1,200 metric tons per month across high-temperature superalloys, precision resistance alloys, and corrosion-resistant grades, securing fast lead times for high-volume enterprise contracts.
  • End-to-End Internal Quality Verification: Every batch of 25mm GH2747 round bars undergoes 100% full-length ultrasonic flaw detection, eddy current inspection, and direct-reading optical emission spectrometry to confirm zero internal voids, inclusions, or chemical segregation.
  • Custom Metallurgy & Tailored Dimensions: Full OEM flexibility in customized chemistries, tight outer-diameter tolerances, specialized mechanical hardening, chamfering, and customized cut-to-length dimensions.
  • Traceable Factory Inspection Certificates: Comprehensive quality test documentation—including actual chemical melt reports, room/high-temperature tensile test records, hardness profiles, and dimensional verification data—is supplied with each shipment.
  • Heavy-Duty Export Packaging: Standard protective rust-inhibiting wrapping, heavy-duty wooden crates, and secure banding ensure zero mechanical distortion or surface abrasion during international maritime and air transit.

production plant

company profile

Frequently Asked Questions

Q1: What are the primary operating temperature boundaries for GH2747 round bars?

A: GH2747 is engineered to withstand continuous operating temperatures up to 1200°C and intermittent peak excursions up to 1250°C, demonstrating far superior oxidation resistance compared to conventional heat-resistant austenitic stainless alloys.

Q2: What is the minimum order quantity (MOQ) and production lead time for 25mm GH2747 bars? 

A: Our standard trial order MOQ starts from 50 kg for in-stock billet re-drawing, while dedicated custom melt batches typically require 200–500 kg depending on dimensional requirements. Standard production lead time ranges between 15 to 30 working days from technical sign-off.

Q3: How does DLX verify the internal integrity and surface quality of 25mm round bars? 

A: All round bars undergo 100% automated ultrasonic internal testing (UT) and surface defect inspection. Surface roughness is inspected with high-precision profilometers, and chemical compositions are certified using high-resolution spark OES spectrometers.

Q4: Can you provide custom cut lengths and specific surface finishes? 

A: Yes. We offer precision band-saw cutting to customized lengths from 50 mm to 6000 mm with deburred or chamfered ends. Surface treatments include black forged, hot-rolled pickled, smooth peeled, or centerless mirror ground (Ra ≤ 0.8 μm).

Q5: What documentation accompanies international bulk shipments?

A: Every shipment includes an official comprehensive Mill Test Certificate (MTC) detailing exact heat-number traceability, chemical composition analysis, room-temperature tensile/yield data, hardness measurements, dimensional inspection logs, and non-destructive testing reports.