Nimonic 90 Pyromet 90 Udimet 90 High Temperature Aluminium Alloys

Contact me for free samples and coupons.
WhatsApp:0086 18588475571
WeChat: 0086 18588475571
skype: sales10@aixton.com
If you have any concern, we provide 24-hour online help.
xProduct Name | Nimonic 90 | Material | Nickel Chromium |
---|---|---|---|
Density | 8.18g/cm³ | Melting Point | 1370°C |
Coefficient Of Expansion | 12.7 μm/m °C (20 – 100°C) | Modulus Of Rigidity | 82.5 KN/mm² |
Modulus Of Elasticity | 213 KN/mm² 227 / 240 KN/mm² | ||
Highlight | Nimonic 90 High Temperature Aluminium Alloys,Pyromet 90 High Temperature Steel,Udimet 90 High Temperature Aluminium Alloys |
- Nimonic 90high temperature nickel alloy
Nimonic 90 wire, A Nickel-Chromium-Cobalt alloy being precipitation hardenable, having high stress-rupture strength and creep resistance at high temperatures up to about 950oC (1740oF). It is widely used and a well proven alloy in high temperature conditions.
Nimonic 90 is also known as Superimphy 90, Pyromet 90, and Udimet 90.
-
Nimonic 90 wire Chemical Composition
The chemical composition of Nimonic 90 wire is given in the following table.
Element | Content (%) |
---|---|
Nickel, Ni | Bal |
Chromium, Cr | 18-21 |
Iron, Fe | ≤1.5 |
Cobalt, Co | 15-21 |
Titanium, Ti | 2-3 |
Aluminum, Al | 1.0-2.0 |
Manganese, Mn | ≤1 |
Silicon | ≤1 |
Others | Remainder |
-
Nimonic 90 Physical Properties
The following table discusses the physical properties of Nimonic 90.
Properties | Metric | Imperial |
---|---|---|
Density | 8.18 gm/cm3 | 0.296 lb/in3 |
-
Nimonic 90 Mechanical Properties
The mechanical properties of Nimonic 90 wire are tabulated below.
Properties | ||||
---|---|---|---|---|
Condition | Approx. tensile strength | Approx. operating temperature depending on load^^ and environment | ||
N/mm² | ksi | °C | °F | |
Annealed | 800 – 1000 | 116 – 145 | – | – |
Annealed + Aged | 1200 – 1400 | 174 – 203 | up to 550 | up to 1020 |
Spring Temper | 1200 – 1500 | 175 – 218 | – | – |
Spring Temper + Aged | 1500 – 1800 | 218 – 261 | up to 350 | up to 660 |