xProduct Name | Nimonic 80A | Material | Nickel Chromium |
---|---|---|---|
Density | 8.37g/cm³ | Melting Point | 1380°C |
Coefficient Of Expansion | 11.0 μm/m °C (20 – 100°C) | Annealed | 700 – 800N/mm² |
Spring Temper | 1200 – 1500N/mm² | ||
Highlight | Nimonic 75 High Temperature Nickel Alloy,N06075 Hi Temp Alloys,ISO 9001 Wire High Temperature Nickel Alloy |
- NIMONIC alloy 75 High Temperature Nickel Alloy
NIMONIC alloy 75 Alloy 75 (UNS N06075, Nimonic 75) rod is a 80/20 nickel-chromium alloy with controlled additions of titanium and carbon. Nimonic 75 has good mechanical properties and oxidation resistance at high temperatures. Alloy 75 is most commonly used for sheet metal fabrications which require oxidation and scaling resistance together with medium strength at high operating temperatures. Alloy 75 (Nimonic 75) is also used in gas turbine engines, for components of industrial furnaces, for heat treating equipment and fixtures, and in nuclear engineering.
-
Nimonic 75 Chemical Composition
The chemical composition of NIMONIC alloy 75 is given in the following table.
Element | Content (%) |
---|---|
Nickel, Ni | Bal |
Chromium, Cr | 19-21 |
Iron, Fe | ≤5 |
Cobalt, Co | ≤5 |
Titanium, Ti | 0.2-0.5 |
Aluminum, Al | ≤0.4 |
Manganese,Mn | ≤1 |
Others | Remainder |
-
Nimonic 75 Physical Properties
The following table discusses the physical properties of NIMONIC alloy 75.
Properties | Metric | Imperial |
---|---|---|
Density | 8.37 gm/cm3 | 0.302 lb/in3 |
-
Nimonic 75 Mechanical Properties
The mechanical properties of NIMONIC alloy 75 are tabulated below.
Properties | ||||
---|---|---|---|---|
Condition | Approx. tensile strength | Approx. operating temperature depending on load** and environment | ||
N/mm² | ksi | °C | °F | |
Annealed | 700 – 800 | 102 – 116 | -200 to +1000 | -330 to +1830 |
Spring Temper | 1200 – 1500 | 174 – 218 | -200 to +1000 | -330 to +1830 |